Dear all
Interpretation: IX-92-70R
Subject: QW-403.5, Base Metals
Date Issued: June 4, 2001
File No: 00-470
Question (3): When a procedure qualification with supplemental notch toughness requirement is conducted with two materials of different P-Number each having multiple certifications in different Group Numbers, are WPSs qualified for all combinations of the multiple certified Group Number of the first P-Number material to the multiple certified Group Number of the second P-Number material?
Reply (3): Yes.
Interpretation: IX-89-75
Subject: Section IX; QW-403.5, QW-403.11, and QW-424
Date Issued: September 20, 1990
File: BC90-443
Question (1): A procedure qualification using the SMAW process in a V-groove joint has been qualified with acceptable bends, tensiles and charpy V-notch impact specimens, using P-No. 1 Group 2 material welded to a P-No. 3 Group 3 material. Does the procedure qualification support the welding of P-No. 1 Group 2 material together when notch toughness tests are required?
Reply (1): No.
Question (2): Does the procedure qualification support the welding of P-No. 1 Group 2 material to P-No. 3 Group 3 material?
Reply (2): Yes.
Question (3): Does the procedure qualification support the welding of P-No. 3 Group 3 material together?
Reply (3): No
What is the difference between two statements? Kindly explain
Interpretation: IX-92-70R
Subject: QW-403.5, Base Metals
Date Issued: June 4, 2001
File No: 00-470
Question (3): When a procedure qualification with supplemental notch toughness requirement is conducted with two materials of different P-Number each having multiple certifications in different Group Numbers, are WPSs qualified for all combinations of the multiple certified Group Number of the first P-Number material to the multiple certified Group Number of the second P-Number material?
Reply (3): Yes.
Interpretation: IX-89-75
Subject: Section IX; QW-403.5, QW-403.11, and QW-424
Date Issued: September 20, 1990
File: BC90-443
Question (1): A procedure qualification using the SMAW process in a V-groove joint has been qualified with acceptable bends, tensiles and charpy V-notch impact specimens, using P-No. 1 Group 2 material welded to a P-No. 3 Group 3 material. Does the procedure qualification support the welding of P-No. 1 Group 2 material together when notch toughness tests are required?
Reply (1): No.
Question (2): Does the procedure qualification support the welding of P-No. 1 Group 2 material to P-No. 3 Group 3 material?
Reply (2): Yes.
Question (3): Does the procedure qualification support the welding of P-No. 3 Group 3 material together?
Reply (3): No
What is the difference between two statements? Kindly explain