Joint configuration is an essential variable as per QW-288 in Section IX.
Can Groove plus fillet weld procedure be applied to fillet weld only production joint provided all other essential variables are not changed?
QW-288 does not talk about fillet welds, it only addresses groove joint.
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
Can Groove plus fillet weld procedure be applied to fillet weld only production joint provided all other essential variables are not changed?
QW-288 does not talk about fillet welds, it only addresses groove joint.
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN