QW-200.4 of ASME Sec. IX_Combination of Welding Procedures

Status
Not open for further replies.

sushildwivedi16

Materials
Joined
Aug 20, 2015
Messages
14
Location
AE
Hello Everyone,

This is my first post here. Hope to find the solution to my query with respect to QW-200.4 of ASME Sec. IX.

Here I go!!

PQR A is qualified in 25 mm base metal thickness with 10 mm of GTAW & 15 mm of SMAW weld deposits. PQR B is qualified in 8 mm base metal thickness with 3 mm of GTAW & 5 mm of SMAW weld deposits. In both the PQRs, the tensile and bend tests have been carried out satisfactorily.

Can I generate a single WPS of GTAW process only with base metal thickness range as 1.5-50 mm, GTAW weld deposit max thickness - 20 mm ?

The production joint thicknesses are 4.55 mm and 12 mm and do not require impact testing and have to be welded entirely with GTAW process only.

Also can I generate a second WPS of GTAW+SMAW process with base metal thickness range as 1.5-50 mm, GTAW weld deposit max thickness - 20 mm, SMAW process weld deposit max thickness - 30 mm ?

Thanks to all in advance.
 
Please do not post in other forums, you have your answer

thread330-408965
 