We have to qualify tube to tube sheet joint in accordance with ASME Section IX.
Joint is groove plus fillet type. Groove depth is 7 mm and fillet leg size is 3 mm.
QW-193.1.3(a) talks about "Minimum Leak Path Dimension", in the above case is it 7+3=10 mm?
I interpret "minimum leak path dimension" as the distance fluid covers if it were leaking. So it covers 10 mm distance if it were leaking. Please advise.
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
Joint is groove plus fillet type. Groove depth is 7 mm and fillet leg size is 3 mm.
QW-193.1.3(a) talks about "Minimum Leak Path Dimension", in the above case is it 7+3=10 mm?
I interpret "minimum leak path dimension" as the distance fluid covers if it were leaking. So it covers 10 mm distance if it were leaking. Please advise.
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN