Hi everybody,
I'm facing an issue in motors where some Copper parts have become "Pink"....But a real bright Pink. Have any of you ever faced this kind of problem?Would you know what could be the cause (Heat(doubt it even if the motor is fairly hor never seen that before)?Corrosion?Pollution??).
Thank you very much for your help!!!
I'm facing an issue in motors where some Copper parts have become "Pink"....But a real bright Pink. Have any of you ever faced this kind of problem?Would you know what could be the cause (Heat(doubt it even if the motor is fairly hor never seen that before)?Corrosion?Pollution??).