Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

"ASTM A193 Gr B7" Hydrochloric acid service

Status
Not open for further replies.

shahyar

Chemical
Feb 15, 2005
216
Hi,
On a FRP tank for Hydrochloric acid 32% in ambient temperature, we proposed Hastelloy, but vendor says:"ASTM A193 Gr B7" for stud bolts. Which is better material?
(Outdoor tank, min Amb. Temp = minus 45 deg C)

Regards
 
Replies continue below

Recommended for you

Will the bolts be wet by the acid or fumes? If so, they won't be bolts for long-they're low-alloy steel like 4140. Which Hast. would be used?
 
B7 No; Hastelloy C Yes.
We also use a lot of Silicon Bronze in this service for flange bolting, especially in the smaller sizes.
 
PTFE-coated B7 studs and 2H nuts are commonly used, temperature permitting. Forget about Hastelloy bolting- $$$ and galling tendency will both be enormous.
 