When you are told that you are using 350W steel, what does the 350 represent? What does the W represent?

Its a study question, but just wanted to run it by you guys so i know i am correct.

W represents that the steel is weldable

350 describes the nominal depth(feel like i am wrong on this one?!)



Thanks in advance.
 
W means it's weldable...
 
Quick responses are quick.

Thx
 
Grade 350W is weldable steel with a yield stress of 350 MPa.
A W350x## section is a wide flange beam with a depth of 350 mm.
 
Thanks Trundle for making that more clear.
 