Hi,
I am rebuilding a foundation under a natural gas pipeline compressor. We will use rebar, anchor bolt canisters, and steel oil pan. The foundation will be approximately 15-18 yds, and formed with the compressor in place supported by jacks. The compressor plant will have 7 other compressors running and vibration and cracking is an issue. We would like the repaired foundation to last another 50 years. Downtime is also an issue. We will use an epoxy grout on top of the concrete to hold sole plates for the compressor in place.
What are the problems with with high early that I should be aware of?
What are the problems assosiated with calcium cloride in concrete?
Is thermal cracking from curing a problem?
I am rebuilding a foundation under a natural gas pipeline compressor. We will use rebar, anchor bolt canisters, and steel oil pan. The foundation will be approximately 15-18 yds, and formed with the compressor in place supported by jacks. The compressor plant will have 7 other compressors running and vibration and cracking is an issue. We would like the repaired foundation to last another 50 years. Downtime is also an issue. We will use an epoxy grout on top of the concrete to hold sole plates for the compressor in place.
What are the problems with with high early that I should be aware of?
What are the problems assosiated with calcium cloride in concrete?