My customer has asked me to increase a distance between two welds on a pipe at least 50mm(welded toe to toe), which is now 45mm from each welding center as shown in the attached picture.
Unfortunately, the distance cannot be increased anymore due to several reasons. I therefore am trying to find a way to persuade the customer to keep the current condition.
It would very helpful to me if you could let me have answers to the followings:
* Pipe info.
- Pipe size: 250A(Thickness: 9.3)
- Pipe mat'l: Carbon steel (JIS CODE: STPG370-ERW)
- Medium: Lub. Oil (Working pressure: under 3 bar)
- Welding: Butt welding
* What I need to know
1) Is there any possibility to overlap HAZ of each welds? How can I calculate width of HAZ?
2) If HAZ is overlapped, What problem occur?
3) What should I do to verify integrity of the pipe? Welds penetrant test alone is enough to verify? or is any other examination necessary?
Hyunik Cho
HYUNDAI Engineering & Technology
Ulsan, South Korea
Unfortunately, the distance cannot be increased anymore due to several reasons. I therefore am trying to find a way to persuade the customer to keep the current condition.
It would very helpful to me if you could let me have answers to the followings:
* Pipe info.
- Pipe size: 250A(Thickness: 9.3)
- Pipe mat'l: Carbon steel (JIS CODE: STPG370-ERW)
- Medium: Lub. Oil (Working pressure: under 3 bar)
- Welding: Butt welding
* What I need to know
1) Is there any possibility to overlap HAZ of each welds? How can I calculate width of HAZ?
2) If HAZ is overlapped, What problem occur?
3) What should I do to verify integrity of the pipe? Welds penetrant test alone is enough to verify? or is any other examination necessary?
Hyunik Cho
HYUNDAI Engineering & Technology
Ulsan, South Korea