I have a soil with a LL=181 PL=136 PI=45
some type of volcanic ash... we are running a proctor and getting some unexpected results.
pt1 max den=29.5pcf m%=146
pt2 max den=35.5pcf m%=128
pt3 max den=32.5pcf m%=118
the field moisture was 180%+ so we have been drying it running the tests along the way.
so according to this the max dry dens is around 35.9pcf and m% 131.5
is that reasonable? im gonna keep drying it out and see what happens.
some type of volcanic ash... we are running a proctor and getting some unexpected results.
pt1 max den=29.5pcf m%=146
pt2 max den=35.5pcf m%=128
pt3 max den=32.5pcf m%=118
the field moisture was 180%+ so we have been drying it running the tests along the way.
so according to this the max dry dens is around 35.9pcf and m% 131.5
is that reasonable? im gonna keep drying it out and see what happens.