mariolucas75
Civil/Environmental
Dear Forum members please help with one easy question from B31.3 pipe thickness calculation.
I am preparing myself for an exam to take API570.
This is one of the questions I encountered and got stuck:
An NPS 4(4.5” o.d.) seamless pipe made from ASTM A-106 Grade A material operates at 300 psi and 400 degrees F. The pipe must cross a small ditch and it must be capable of supporting itself without any visible sag. A piping Engineer states that the pipe must be at least 0.25” thick just to support itself and the liquid product. He also states that a 0.10” corrosion allowance must be included. Calculate the thickness required for the pipe.
a. 0.292”
b. 0.392”
c. 0.350”
d. 0.142”
The answer sheets says that the correct answer is b 0.392 referring to B31.3,304.1.2 (a).
But when I use that formula to calculate the thickness I get 0.0418” for pressure design thickness.
If we add 0.1” for corrosion allowance we get for minimum required thickness 0.1418”.
Since the exam question above says that min required thickness is 0.25” that is thicker then calculated value so we can pick the nearest value to 0.25 from the given variants and which logically is 0.292”.
However the answer sheet says 0.392”.
Could you please help me why is that?
Thanks so much.
I am preparing myself for an exam to take API570.
This is one of the questions I encountered and got stuck:
An NPS 4(4.5” o.d.) seamless pipe made from ASTM A-106 Grade A material operates at 300 psi and 400 degrees F. The pipe must cross a small ditch and it must be capable of supporting itself without any visible sag. A piping Engineer states that the pipe must be at least 0.25” thick just to support itself and the liquid product. He also states that a 0.10” corrosion allowance must be included. Calculate the thickness required for the pipe.
a. 0.292”
b. 0.392”
c. 0.350”
d. 0.142”
The answer sheets says that the correct answer is b 0.392 referring to B31.3,304.1.2 (a).
But when I use that formula to calculate the thickness I get 0.0418” for pressure design thickness.
If we add 0.1” for corrosion allowance we get for minimum required thickness 0.1418”.
Since the exam question above says that min required thickness is 0.25” that is thicker then calculated value so we can pick the nearest value to 0.25 from the given variants and which logically is 0.292”.
However the answer sheet says 0.392”.
Could you please help me why is that?
Thanks so much.