I have an application where I need to glue a glass disc to the end of a steel shaft.
The assembly needs to withstand 120°C. Can anyone recommend a good adhesive for this purpose?
 
Replies continue below

Recommended for you

Most adhesives would work okay. Epoxy or silicone would be good choices.
 
The alternative is to metallize the glass, then solder the disc to the steel.
 