we use QZ110 quartz with ER450 epoxy matrix for some project. i cant find any info about QZ110 prepreg. we got this material from a reseller without any COC. due to some end user statements information like mechanical properties can not be provided to us.
we do all the mechanical tests by ourself but i have nothing yo compare my results with.
does anyone familiar with that prepreg?
 
Also can't find QZ110. If it's quartz (pure silica) then according to Saint Gobain it should have the same properties as E-glass in decent resins. Your resin looks ok if it's the stuff from Saati. I can't find the Saint Gobain data online so I attach it.
 
 http://files.engineering.com/getfile.aspx?folder=57714902-4e8d-47a8-a2af-944f1062207c&file=Saint-Gobain_Quartzel_Brochure_and_Technical_Data.pdf