Hi there,
We are making some parts of carbon fiber with prepreg. We are using Sigrapreg E323.
We do a cycle at 80ºC (176ºF) 1,5 hours and then another one at 120ºC (248ºF) another 1,5h.
The timer of the oven didn't work so it cured the second cycle at 120ºC during 18 hours.
Is this a problem? Is there such a thing like "overcuring"?
thanks
regards
We are making some parts of carbon fiber with prepreg. We are using Sigrapreg E323.
We do a cycle at 80ºC (176ºF) 1,5 hours and then another one at 120ºC (248ºF) another 1,5h.
The timer of the oven didn't work so it cured the second cycle at 120ºC during 18 hours.
Is this a problem? Is there such a thing like "overcuring"?
thanks
regards