C37700 is limited to 200 F maximum. In order to increase the design allowable to 425 F, you will have to initiate and submit a Code Case defining the design allowable from 200 to 425F. You will need the support of the material's manufacturer(s). You should first consider the selection of an alternate material unless C37700 is the only material which can meet the service. And I do speak from experience.