Hii everyone...in ASME sec9, part QW423, a welder qualified with P no=1 can weld P No 1 to 11 ...does this include p no's 5A and 5B...thanks
 
emrekop,
Be careful, base metal substitution can only be done if all other essential variables in the WPS/PQR being used remain the same. I've seen this paragraph misapplied more than once.
Regards,
RLS
 