Aug 14, 2012 #1 Aliq298 Industrial Joined Dec 29, 2011 Messages 16 Location MY All, May i Qualified the 2 welder using only 1 test coupon according to AWS D1.1? which clause i should refer to?? Please Advise.
All, May i Qualified the 2 welder using only 1 test coupon according to AWS D1.1? which clause i should refer to?? Please Advise.
Aug 14, 2012 #2 Ron Structural Joined Sep 24, 1999 Messages 16,336 Location US No. One coupon per welder. Upvote 0 Downvote
Aug 14, 2012 Thread starter #3 Aliq298 Industrial Joined Dec 29, 2011 Messages 16 Location MY Thanks ron, But which clause i should refer to..because AWS D1.1 doesn't show at essential for welder. Maybe u can give me the hint why can't... Just seekig some advise. newbie engineer Upvote 0 Downvote
Thanks ron, But which clause i should refer to..because AWS D1.1 doesn't show at essential for welder. Maybe u can give me the hint why can't... Just seekig some advise. newbie engineer