Hi,

What is de T range if:

SMAW - Plate 15 mm - V-groove - P6 - PWHT and Impact tested in PQR

Table QW-451.1 ASME IX said: Over 3/8 (10), but less than 3/4 (19) = 2T for T for base metal.

Someone told me that T = 1.1 x T because Impact test and PWHT performed during the PQR

Is that so and where is this described in te ASME IX?

Thnx!
Patrick
 
Replies continue below

Recommended for you

Please do not cross post threads.

thread794-358907
 