Please. Anybody can explain in ASME sec viii dev.1 table UCS-56 point 3a
 
RVinothkumar, you need to specify which Table, there are eleven. Full description of the Note, e.g. (b)(3)(a).

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
RVinothkumar, this note exempts PWHT of certain welds which would otherwise be required by the service requirements of UW-2. Specific to certain small connections. Other exemptions follow.

Regards,

Mike