Dear All
We are using 20 mm thick plate for Shell and 20 mm plate for Nozzle Reinforcement pad.
As we are giving full penetration weld in nozzle to Shell groove and Shell to Pad groove(total welding is 40 mm), kindly clear whether PWHT requirement is there or not.
We are using 20 mm thick plate for Shell and 20 mm plate for Nozzle Reinforcement pad.
As we are giving full penetration weld in nozzle to Shell groove and Shell to Pad groove(total welding is 40 mm), kindly clear whether PWHT requirement is there or not.