Let’s be clear about this - if weld repairs are performed to the NBIC, the repair welds only would require PWHT based on original code of construction PWHT requirements for fabrication welds. The NBIC does not provide requirements for code of construction PWHT. The NBIC defaults back to the original code of construction for repair welds unless PWHT for technical reasons cannot be performed because of harm to the vessel itself. In this case, if the original code of construction required PWHT because of material composition and thickness, the repair welds would require PWHT.
The same also holds true for NDT, unless other options are evaluated by the Inspector and, if necessary, from the Jurisdiction.