Is there an actual ASME code limiting the number of times I can PWHT WC6 P4 material? Any help on this subject would be greatly appreciated.
 
Replies continue below

Recommended for you

Possibly - how is that for an ASME response?

If the application of the casting requires impact testing per a specific Code or Standard, cumulative PWHT time becomes an essential variable because this will affect impact properties.

If impact requirements are not specified, you can repair a casting as many times as necessary OR unless the purchaser has specified in the PO a limit as to the number of weld repairs.
 
Thanks metengr, there is not any impact testing for this part. Thanks again
 