I'm sure the question has been asked before, but what is the minimum hold time for PWHT on P91? The question is pertinent to thin sections (1/2" and lower say).
I believe ASME VIII (UCS-56) suggests it is possible to do as little as 15 mins on thin sections (<1/4"). However, I've seen some guidance, including:
and
Suggesting 2 hr min on the basis to ensure complete tempering.
Is anyone able to advise?
Regards
kclim
I believe ASME VIII (UCS-56) suggests it is possible to do as little as 15 mins on thin sections (<1/4"). However, I've seen some guidance, including:
and
Suggesting 2 hr min on the basis to ensure complete tempering.
Is anyone able to advise?
Regards
kclim