I am working on a project to add some nozzles to vertical drums. Both of them were built in 1975 and the shell material is SA-285-C.
I have some confusion regarding the Post Weld Heat Treatment of the vessels. One has a 1-9/16" thick shell and the other has a 1-5/8" thick shell. The manufacturers data reports indicate that neither vessel was heat treated. According to table UCS-56, SA-285-C should be heat treated if its thickness is greater that 1-1/2"
Does anyone know of a reason why these vessels would not have been heat treated.
Any advice is greatly appreciated.
I have some confusion regarding the Post Weld Heat Treatment of the vessels. One has a 1-9/16" thick shell and the other has a 1-5/8" thick shell. The manufacturers data reports indicate that neither vessel was heat treated. According to table UCS-56, SA-285-C should be heat treated if its thickness is greater that 1-1/2"
Does anyone know of a reason why these vessels would not have been heat treated.
Any advice is greatly appreciated.