payaam2000
Mechanical
Dear All
we are subjected to a vessel with data below:
SA350 lf2 + 7mm inconel625 overlay
asme sec Viii div 1
Base metal thickness is 45mm
sour service.
nozzle: sa350lf2 + 7 mm inconel625 overlay (8")
now shell has been fabricated (a350 + inconel 625 overlay)
vendor is going to weld nozzles on the shell with deep groove figure
my question is that when nozzle welded to shell , should vessel to be subjected to PWHT?
if yes, doesn't it any harmful effect on inconel weldedoverlay.
again if yes, doesn't it create separation of inconel and carbon steel layers along with interface zone (because of different thermal expansion coefficient of inconel and a350)?
best regards
we are subjected to a vessel with data below:
SA350 lf2 + 7mm inconel625 overlay
asme sec Viii div 1
Base metal thickness is 45mm
sour service.
nozzle: sa350lf2 + 7 mm inconel625 overlay (8")
now shell has been fabricated (a350 + inconel 625 overlay)
vendor is going to weld nozzles on the shell with deep groove figure
my question is that when nozzle welded to shell , should vessel to be subjected to PWHT?
if yes, doesn't it any harmful effect on inconel weldedoverlay.
again if yes, doesn't it create separation of inconel and carbon steel layers along with interface zone (because of different thermal expansion coefficient of inconel and a350)?
best regards