Hello All ,
Carbon Steel Vessel : SA 516 70
Cladding : 316L (For corrision resistance)
Service : H2S
Thickenss of Vessel : 18 mm
CA for CS : .125" and SS : .0625"
Is PWHT is required for this vessel ? I know that the thickness is within limits , but since the service is H2S , may be PWHT is required , I have checked section UCS , but didnt find the solution . Can any one give suggestions.
BR
Assad
Carbon Steel Vessel : SA 516 70
Cladding : 316L (For corrision resistance)
Service : H2S
Thickenss of Vessel : 18 mm
CA for CS : .125" and SS : .0625"
Is PWHT is required for this vessel ? I know that the thickness is within limits , but since the service is H2S , may be PWHT is required , I have checked section UCS , but didnt find the solution . Can any one give suggestions.
BR
Assad