Oct 30, 2006 #1 SJones Petroleum Joined Apr 22, 2001 Messages 3,951 Location GB thread794-169240 Just to keep answers in one place! Thanks. Steve Jones Materials & Corrosion Engineer http://www.pdo.co.om/pdo/
thread794-169240 Just to keep answers in one place! Thanks. Steve Jones Materials & Corrosion Engineer http://www.pdo.co.om/pdo/
Oct 30, 2006 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US SJones; Have you seen this article below? http://www.specialmetals.com/products/incoloyalloy825.htm Upvote 0 Downvote
Oct 30, 2006 1 Thread starter #3 SJones Petroleum Joined Apr 22, 2001 Messages 3,951 Location GB Yes I have thanks; however, it was Figure 1 in this one: http://thyssenkruppvdm.de/_pdf/Nicrofer_4221_e.pdfthat is the subject of my interest. Steve Jones Materials & Corrosion Engineer http://www.pdo.co.om/pdo/ Upvote 0 Downvote