Dear all,

in case of Nozzle-To-Shell attachment in a configuration like that stated in Fig. UG-40(b-1) of ASME VIII-1 (Ed. 2007 an successive), whick is the definition of the "thickness" (t.PWHT) to be considered in PWHT CODE ASSESMENT (by CODE)?

Some Client/ASME Inspectors assume a "more conservative assumption" like:

t.PWHT = ( te + t.Shell )

others assume a "more light assumption" like

t.PWHT = MAX (te; t.Shell)

Please also refer to UW-40(f)(5)(d) - The source of the "dilemma".

NOTE: I was not able to find out any "clarification" on this issue, nor any "interpretation".

NOTE: some time we "shift" the nozzle-to-shell details to that shown in Fig. UW-16.1(h) of ASME VIII-1: thsi detail is classified as a FULL PENETRATION WELD ATTACHMENT (in this way, t.PWHT become clear and univoque).

See also Par. UW-16(c)(2)(d).

Does someone have more experience to share on this issue?

Many thanks in advance.

ANN
 
Replies continue below

Recommended for you

The definition of nominal thickness for PWHT of ASME Section VIII, Div 1 fabrication can be found in UW-40 8(f) 5 (d).
 