PWHT MULTIPLE TIMES ON THE SAME JOINT OF SA335P91 MATERIAL

ishtechmech

Mechanical
Joined
Jun 19, 2012
Messages
4
Location
IN
How many times PWHT one can perform on SA2335P91 Joints ? what issue may arise if we do PWHT multiple times on such joints . give scientific reasons.

what if the material is carbon steel or low alloy steel?
 
How many times is a multiple for you? 3, 5, 10?
Give scientific reasons.
 
I limited it to 2 and then required a full cut out and reweld. Excessive surface decarburization was the main reason plus over tempering. In one instance I required pipe spools to be cut out and reheat treated in vacuum furnaces after evaluating microstructure.
 
With an alloy like 91 where the creep properties are strongly changed by HT you have to be careful.
Changes in the microstructure will have risks.
You can use multiple PWHT as long as you have verified the resulting properties.
 
How can you check the desired properties after PWHT?
 
I insist.
How to check if the PWHT was correct and produced the desired result?
It seems no one has experience in manufacturing and inspection
If someone specifies PWHT, they should know how to check it.
 
There have been a number of reports/studies published by EPRI on this subject. I believe they are still free. There has been much research published with regard to P91 and its manufacture and heat treatment and welding thereof.
 
It is very easy to check the PWHT, I did it a few years ago.
 
It seems the PWHT has been rejected...was there a failure of the heating coils or the power source during treatment?
Did the chart did not conform to the heat treatment cycle?
Or did you get hardness values outside limits?
Answers to above would help to reach a solution.
 