Hello everybody
as subject, I have many joints Olet (weldolet/Nipoflange) are seft reinforement more than 25mm welded to pipe run 10''SCH80(15.09mm) & 12"SCH80(17.48). As per ASME B31.3 2014 defined that Tm+Tc>25mm in FIG.328.5.4F is need to PWHT or preheat 95deg without PWHT. but currently we are used WPS qualified by PWHT.
my question: Do we need to perform PWHT in case?
as subject, I have many joints Olet (weldolet/Nipoflange) are seft reinforement more than 25mm welded to pipe run 10''SCH80(15.09mm) & 12"SCH80(17.48). As per ASME B31.3 2014 defined that Tm+Tc>25mm in FIG.328.5.4F is need to PWHT or preheat 95deg without PWHT. but currently we are used WPS qualified by PWHT.
my question: Do we need to perform PWHT in case?