Does anyone have experience using PVDF Impeller-Driven Pumps and how reliable they are? I was hoping to find some data or research article on it. Thanks!
Just like all polymer pumps, they work fine.
But they are very sensitive to the operating limits.
Any slight overload or over temperature and you are likely to destroy them.
And the real key is what is the reinforcement?