here's the important bit of the abstract (my bold)
Published data on photovoltaic (PV) degradation measurements were aggregated and re‐examined. The subject has seen an increased interest in recent years resulting in more than 11 000 degradation rates in almost 200 studies from 40 different countries. As studies have grown in number and size, we found an impact from sampling bias attributable to size and accuracy. Because of the correlational nature of this study we examined the data in several ways to minimize this bias. We found median degradation for x‐Si technologies in the 0.5–0.6%/year range with the mean in the 0.8–0.9%/year range.
So they had some dreadful panels, dragging the mean down. 0.6%/year gives a drop in output of 12% over 20 years.
Cheers
Greg Locock