rvidal
Structural
- May 13, 2003
- 1
Today I found myself confused as to IF ss piping (304 specifically) needed to be purged prior to welding. There is a project in the shop, pre-fab of a vapor piping, 2" sch40 304 ss for a local food plant ( no inspection required) and it is not being purged. Also, the first pass is fusion welded (no penetration whatso ever) and My boss's point of view is that the purging is not required because it is for vapor, and that the client know's that it is not being purged prior to welding; He is telling me also that there are 30 year old installations that were welded the same way and are functional ( he went into detail about engineering economics as to say that It would not be cost effective to purge). I strongly dissagree, but this may be because of my ignorance to some aspects of ss. I have studied guides of ss welding, I am a Certified Welding Inspector and I don't remember ever wleding without purging on SS
Appreciate any responses
regards
Raul
Appreciate any responses
regards
Raul