Transient1
Mechanical
I need to select an appropraite snubber material for use in an electronics box that will be flown in space (So outgassing is an issue). I've been trying to a find a listing of viscoelastic materials or a supplier for circuit board snubbers and google has been coming up with very little. So far I've gathered that Solithane and Urethane may be appropriate materials. I'm not sure if the silcon based pads can be cut and if there are any issues with outgassing. Does anyone on the forum know of any suppliers out there that might just have a list of materials and some basic properties? The snubbers I would need would be in the form of short (1'' to 2'') thick strips long and (.25''-.5'') square.