Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Punching shear check

Status
Not open for further replies.

Sbander

Civil/Environmental
Feb 20, 2002
3
Is the punching shear check right on SAFE Specially for corner & edge column?
 
Replies continue below

Recommended for you

hi

i modeling a mat foundation in safe02000 but in punching control i think it is fals because 80 cm thikness need to contorol of punch shear!
meysam jalali-iran-shahrood university
my mail:mei_jalali@yahoo.com
please connect to me.
thanks.
 
Hello guys:

Remember you have to provide at least d/2 clearance off the column so it can check shear. If you fail to provide this off the face of the column you will get a n/c at that joint.

For example if you have an 80 cm mat you ought to give a clearance of 40 cms at least from the face of the load size specified in the software. If you specified a 30 cms size load you need to provide a clearance of 55 cms at least.

Hope this help

Juan
 
CSI have an article "SAFE Technical Note 1" entitled "How SAFE Calculates Punching Shear For the ACI 318-95 Code". This article can be downloaded from the CSI web site.
 