Hi all...
I am working on a project to size a pump for for the following application parameters:
Flow=120GPM
Head=120
Temp=120F
Press=atmospheric
here is the interesting thing: The fluid to be pumped is 10%vol. Caustic soda and 15%vol. Bleach. Is Specific Gravity of 1.2 conservatively good?
Now that I have to select the pump material, is 316SS good for this application?
I am new with the company and my supervisor has business background, so, he left me to decide what is good for this application.
Any comments on my unexperienced conclusions?
Thanks in advance:
I am working on a project to size a pump for for the following application parameters:
Flow=120GPM
Head=120
Temp=120F
Press=atmospheric
here is the interesting thing: The fluid to be pumped is 10%vol. Caustic soda and 15%vol. Bleach. Is Specific Gravity of 1.2 conservatively good?
Now that I have to select the pump material, is 316SS good for this application?
I am new with the company and my supervisor has business background, so, he left me to decide what is good for this application.
Any comments on my unexperienced conclusions?
Thanks in advance: