Gents,
I need your advice for the recommended pump impeller material for duble suction between bearings tar pumps. the existing material is Ductil Iron and the inspection shows sever pin holes on the impeller blades and wearing ring areas. errosion marks on the blade tips (discharge) and sever errosion on the suction eye.
this is a very dirty service as the pump operates on cavitation, PH upset conditions
do you think Bronze will do the job , how it is compared with SS-410, do we need to upgrade the wearing rings as well?
thanks
upm
I need your advice for the recommended pump impeller material for duble suction between bearings tar pumps. the existing material is Ductil Iron and the inspection shows sever pin holes on the impeller blades and wearing ring areas. errosion marks on the blade tips (discharge) and sever errosion on the suction eye.
this is a very dirty service as the pump operates on cavitation, PH upset conditions
do you think Bronze will do the job , how it is compared with SS-410, do we need to upgrade the wearing rings as well?
thanks