sub3marathonman
Computer
The first posting here, so please be kind. I'm somewhat out of my area, which is why I'm hoping the experts will help!
I'm trying to calculate something I never expected to be so complex, the pullout force of an 8mm lag bolt 2" into a pine 2x4. I researched this, and found a formula, using .41 as the specific gravity, on this site: page 8-12. Using that formula, p=8100*G^1.5*D^0.75*L, I come up with 149 lbs for 2 inches of thread penetration. Or just 75 lbs per inch. Which does seem low in my opinion, but I don't know.
However, on this forum, , the pullout strength for a #10 wood screw into southern yellow pine (SYP) was stated, by CJJS, to be 163 lb/inch. And no negative comment implied toward CJJS, it is just that the formula used to calculate the 163 lb/inch of thread penetration wasn't shown. I guess it may be common knowledge among experts, but I'm not an expert, I'm just hoping to try to learn.
So I'm wondering if somebody here could either show me the formula that CJJS used and/or show me where my formula is wrong.
The help is greatly appreciated.
I'm trying to calculate something I never expected to be so complex, the pullout force of an 8mm lag bolt 2" into a pine 2x4. I researched this, and found a formula, using .41 as the specific gravity, on this site: page 8-12. Using that formula, p=8100*G^1.5*D^0.75*L, I come up with 149 lbs for 2 inches of thread penetration. Or just 75 lbs per inch. Which does seem low in my opinion, but I don't know.
However, on this forum, , the pullout strength for a #10 wood screw into southern yellow pine (SYP) was stated, by CJJS, to be 163 lb/inch. And no negative comment implied toward CJJS, it is just that the formula used to calculate the 163 lb/inch of thread penetration wasn't shown. I guess it may be common knowledge among experts, but I'm not an expert, I'm just hoping to try to learn.
So I'm wondering if somebody here could either show me the formula that CJJS used and/or show me where my formula is wrong.
The help is greatly appreciated.