Gents,
Can pullout strength (e.g. of an insert or bolt)of composite be determined by analysis??
 
Only as a very crude approximation: use a conservative interlaminar shear strength times an assumed effective area. Testing is recommended.
 
Thanks SWC,

Question, don't the fibre strength and thickness of the laminate play any part in the pullout strength
 
Yes, but pull-thru strength is a very complicated mix of failure modes. Have tried to correlate several analyses with data without much success, unless one is very conservative with assumptions.
 
Normal load can be applied to surface and then check material permissible stresses and strains. Do you have glass fibers or carbon fibers?
 
ameyad - have you correlated your method to test data? or is it just theoretical?
 
ameyard,
the fibres are carbon fibre in fabric and UD form. Could you be more specific with regards to the material permissible stresses and strains

 