Dear All,
we're experiencing severe errosion on some PTA control valves. The most severe is on the pump recirculation valves which see ~100 pressue drop over the seat with 23% solids content in the slurry flow. These valves are installed on the line after the booster pumps to recirculate flow to the pump when the process line has been switched. Valve trim materials such as Hastelloy, Ti-nitrided st.st. and ceramic have only managed up-times of ~6 months to date. Anyone have positive experience with alternative materials/surface treatments?
Help would be appreciated.
DD.
we're experiencing severe errosion on some PTA control valves. The most severe is on the pump recirculation valves which see ~100 pressue drop over the seat with 23% solids content in the slurry flow. These valves are installed on the line after the booster pumps to recirculate flow to the pump when the process line has been switched. Valve trim materials such as Hastelloy, Ti-nitrided st.st. and ceramic have only managed up-times of ~6 months to date. Anyone have positive experience with alternative materials/surface treatments?
Help would be appreciated.
DD.