Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Properties of Weld Groups 2

Status
Not open for further replies.

osol

Geotechnical
Joined
May 4, 2011
Messages
6
Location
US
I have often seen the Blodgett Table for properties of various weld groups (see attached). I have found it to be very useful, but unfortunately this table only provides properties about the strong axis or 'x-x' axis. I was wondering if a similar table exists out there that has formulas for weak axis bending as well?

Thanks,
Omar
 
 https://files.engineering.com/getfile.aspx?folder=16c6e184-8f49-43d6-84dc-2e44384d6c89&file=Blodgett_Welds_Table.jpg
I don't know if you have Blodgett's 'Solutions to design of weldments' (it's a paperback book that came with 'Design of Weldments') or not.....but it's in there.
 
Thanks, I will check it out. I think my boss might have a copy of that in his office.
 
If he doesn't, I think I can post it. (It's just one page, and I don't see a copyright anywhere.)



 
Properties of various weld groups, including both the X- and Y-axes, are shown in Table 2 on page 2.2-8 of "Design of Welded Structures" by Blodgett.
 
Thanks!
 