Hi,
anybody knows a good reference to find physical and mechanical properties of low-alloy steel ASME SA 350 LF5 (1-2% Ni).
I guess they won't differ too much from those of any C-Mn steel.
Thanks
 
Replies continue below

Recommended for you

The mechanical properties may be quite different, depending on the thermomechanical history as well as the test temperature. Nickel steels will have substantially higher fracture toughness, with the ductile-to-brittle transition moving to lower temperatures.
 
Yes, ASME B&PV code, Section II, Part A and Part D.
 
Thanks Metengr!
I got the same answer from a colleague of mine (I'm not familiar with ASME II-D)
 