Hi,
anybody knows a good reference to find physical and mechanical properties of low-alloy steel ASME SA 350 LF5 (1-2% Ni).
I guess they won't differ too much from those of any C-Mn steel.
Thanks
 
The mechanical properties may be quite different, depending on the thermomechanical history as well as the test temperature. Nickel steels will have substantially higher fracture toughness, with the ductile-to-brittle transition moving to lower temperatures.
 
Yes, ASME B&PV code, Section II, Part A and Part D.
 
Thanks Metengr!
I got the same answer from a colleague of mine (I'm not familiar with ASME II-D)
 