Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Properties of cables 2

Status
Not open for further replies.

csd72

Structural
May 4, 2006
4,574
Does anyone know where I can find E and A properties for typical cables? The information that I have only covers strength properties but this doesnt help in calculating end reaction for a catenary curve.

I am looking at around 1/2" diameter overall for the cable and will specify whatever is readily available in galvanised.



 
Replies continue below

Recommended for you

I believe we use 28,000ksi or 28,500 ksi for the E of P/S strand. My instructor explained that the coiling of the wire in a multi-strand rope causes the effective MOE to drop.
 
Thanks Sliderule that reference was exactly what I was looking for.

Dinosaur,

Thanks for the input, Sliderules reference gives an effective MOE for various cables. For 19 wire strand it gives 19000ksi.
 