I'm looking for temperature dependent properties of several alloys, but surprisingly I'm having the most difficult time with nnealed 1018 steel.

I've checked ASM Handbook and MMPDS-07 and have found basic data for ambient temp but not elevated.

young's modulus
yield strength
tensile strength
poisson's ratio
thermal conductivity
cte
 
All of these except the strength will be exactly the same for any low carbon steel (1005-1020).
There is a ton of data on 1008 and 1020.
Try "High Temperature Property Data: Ferrous Alloys, ASM, ed M.E. Rothman, ISBN: 0-87170-243-6

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 