Hello all,
Can you please tell me where i could find 0.2% proof stress values of A216 WCB as a function of temperature..
also, the kind of materials for which 0.1% proof strength to be accounted in strength calculations.
Thanks in advance.

regards,
sathish.
 
Replies continue below

Recommended for you

The term "proof stress" is not a term used in ASME Section VIII. Would you please so kind as to describe what exactly you mean?

Also, if you are working in the ASME BPV Codes, you should be referring to the ASME version of materials - SA-XXX, as opposed to ASTM A-XXX.
 