this Kind of Graphs ( two Peak ) Are representative of what kind of soils ?
 
Replies continue below

Recommended for you

I've had it with a mixture of 85% flyash and 15% river sand - one peak at a very low water content and another at a higher content.
 
Also happens occasionally with clean fine sands.
 