mschneider2
Chemical
I am trying to determine if ASTM 516-70 is an acceptable option for a dehydration vessel used for ethanol vapor drying at the following conditions:
Temp = 300 F
Pressure = 45 PSI
pH = 5.5
Previous construction has used ASTM 515-70.
Thanks for any help you can provide.
Temp = 300 F
Pressure = 45 PSI
pH = 5.5
Previous construction has used ASTM 515-70.
Thanks for any help you can provide.