I am having a print through problem on a laminate that only shows itself when it is warmed by the sun. The laminate was post-cured to about 170* and has been taken up to that same temp on a regular basis by the sun but still shows print-through above about 120*.
The epoxy laminate is hand-laid and made up of cloth with a layer of surfacing veil and finished with several coats of a polyester primer then two-part poly paint. It is a high quality mirror finish that is flawless at room temp.
I have tried sanding off top-coat, then adding more primer without any success. Does anyone have any ideas what I can do about this?
Thanks for any help.