Sep 29, 2005 #1 koza19 Mechanical Joined Sep 28, 2005 Messages 52 Location US Expect an increase in spring wire (ASTM A227 and ASTM A228). About 450 workers at Ivaco Inc.'s steel-making operation near Hawkesbury, Ont., are off the job after failed contract talks. They supply about 40% off rod to the Spring Industry.
Expect an increase in spring wire (ASTM A227 and ASTM A228). About 450 workers at Ivaco Inc.'s steel-making operation near Hawkesbury, Ont., are off the job after failed contract talks. They supply about 40% off rod to the Spring Industry.